Question : 3 of 53
Marks: +1, -0
The hole concentration in an intrinsic semiconductor is 5×108 m−35 \times 10^{8} \text{ m}^{-3}. When it is doped with certain impurity, the electron concentration becomes 4×1012 m−34 \times 10^{12} \text{ m}^{-3}. Find the new value of the hole concentration. Also identify the type of new semiconductor formed after doping.
[CBSE 2026 55/4/3]
Concept:
In an intrinsic semiconductor ne=nh=nin_e = n_h = n_i. At thermal equilibrium, even after doping, the law of mass action holds: nenh=ni2n_e n_h = n_i^2.
Given:
ni=5×108 m−3n_i = 5 \times 10^{8} \text{ m}^{-3} (hole concentration of the intrinsic semiconductor)
ne=4×1012 m−3n_e = 4 \times 10^{12} \text{ m}^{-3} (after doping)
Solution:
nh=ni2ne=(5×108)24×1012=25×10164×1012=6.25×104 m−3n_h = \dfrac{n_i^2}{n_e} = \dfrac{(5 \times 10^{8})^2}{4 \times 10^{12}} = \dfrac{25 \times 10^{16}}{4 \times 10^{12}} = 6.25 \times 10^{4} \text{ m}^{-3}
Type: After doping nen_e (4×1012 m−34 \times 10^{12} \text{ m}^{-3}) is much greater than nhn_h (6.25×104 m−36.25 \times 10^{4} \text{ m}^{-3}). Electrons are the majority carriers, so the doped semiconductor is n-type (doped with a pentavalent, donor impurity).
Result: New hole concentration =6.25×104 m−3= 6.25 \times 10^{4} \text{ m}^{-3}; the semiconductor is n-type.
Key point: Doping with donors raises nen_e and lowers nhn_h below nin_i, because the product nenhn_e n_h stays equal to ni2n_i^2.